Q.

 Column – I Column – I
A.Nylon - 6pAddition copolymer
B.Buna-sqAddition homopolymer
C.MelmacrCondensation homopolymer
D.TeflonsCondensation copolymer
 ABCD
1.sqpr
2.prqs
3.rpsq
4.rpqs

see full answer

Your Exam Success, Personally Taken Care Of

1:1 expert mentors customize learning to your strength and weaknesses – so you score higher in school , IIT JEE and NEET entrance exams.
An Intiative by Sri Chaitanya

a

2

b

1

c

3

d

4

answer is C.

(Unlock A.I Detailed Solution for FREE)

Best Courses for You

JEE

JEE

NEET

NEET

Foundation JEE

Foundation JEE

Foundation NEET

Foundation NEET

CBSE

CBSE

Detailed Solution

detailed_solution_thumbnail
  • Nylon-6 is obtained by heating caprolactum with water at a high temperature.
Question Image
  • Buna-s  is formed by polymerization of buta–1, 3–diene and styrene is an example of
    copolymer formed by addition polymerization.
  • Question Image
  • Melmac is a condensation co-polymer of melamine and formaldehyde.
  • Solution
  • Teflon is manufactured by heating tetrafluoroethene with a free radical or persulphate catalyst at high pressures through Addition homopolymerization.
  • Question Image
Watch 3-min video & get full concept clarity
score_test_img

courses

No courses found

Ready to Test Your Skills?

Check your Performance Today with our Free Mock Test used by Toppers!

Take Free Test

Get Expert Academic Guidance – Connect with a Counselor Today!

best study material, now at your finger tips!

  • promsvg

    live classes

  • promsvg

    progress tracking

  • promsvg

    24x7 mentored guidance

  • promsvg

    study plan analysis

download the app

gplay
mentor

Download the App

gplay
whats app icon
personalised 1:1 online tutoring