The catalyst in Deacon’s process is
Cu2Cl2
Pt
AlCl3
CuCl2
In Deacon’s process, chlorine is manufactured by the atmospheric oxidation of hydrochloric acid in the presence of cupric chloride catalyst at 400°C.
4HCl+O2→CuCl2Cl2+2H2O ;